Mechanical Properties Metric English Comments
Flexural Modulus 5.515 - 6.895 GPa
799.9 - 1000 ksi
ASTM D790
Arkema Group KYNAR® 370 Polyvinylidene Fluoride (PVDF) Homopolymer - Injection Molding
Characteristics: Natural resin - translucent, off-white hemispheres. Low melt shrinkage, graphite powder filled. High stability in harsh thermal, chemical and ultraviolet environments. High toug..