Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.0410 GPa | 5.95 ksi | method 1, Proc.B; ASTM D-790 |
Multibase Multi-Flex® TPE A 6821 C BLK The burn rate is 1 in/min (25 mm/min) based on ASTM FM VSS 302. Multi-Flex TPE contains Kraton™ G.Data provided by Multibase. |
|||
Flexural Modulus | 0.0410 GPa | 5.95 ksi | ASTM D790 |
Covestro Texin® 5290 Thermoplastic Polyurethane, Polyether-based, Medical
(discontinued **) This grade is in chemical compliance with 21 CFR 177.1680 (Polyurethane Resins) and 177.2600 (Rubber articles intended for repeated use) subject to the limitations of this regulation and any other r.. |
|||
Flexural Modulus | 0.0410 GPa | 5.95 ksi | ASTM D790 |
Covestro Texin® DP7-3006 Thermoplastic Polyurethane, Polyether-based, Aliphatic
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Flexural Modulus | 0.0410 GPa | 5.95 ksi | 1% Secant, ASTM D790 |
ExxonMobil Escorene® LD-722 High EVA Film and Compounding Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.A high vinyl acetate copolymer resin for specialty film and compounding applications. Outstanding heat sealability along with excellent strength pr.. |