Covestro Texin® DP7-3006 Thermoplastic Polyurethane, Polyether-based, Aliphatic  (discontinued **)

Category Polymer , Thermoplastic , Polyurethane, TP , Thermoplastic Polyurethane (TPUR), Polyether Grade
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Covestro Texin® DP7-3006 Thermoplastic Polyurethane, Polyether-based, Aliphatic  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This product was discontinued prior to the separation.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 87
87
ASTM D2240
Tensile Strength, Ultimate 31.0 MPa
4500 psi
ASTM D412
Tensile Strength, Yield 5.00 MPa
725 psi
50% Elongation; ASTM D412
Elongation at Break 425 %
425 %
ASTM D412
Flexural Modulus 0.0410 GPa
5.95 ksi
ASTM D790
Resilience 30
30
% Bayshore Resilience; ASTM D2632
Tear Strength 80.0 kN/m
456 pli
Die C; ASTM D624
Taber Abrasion, mg/1000 Cycles 60
60
H-18 Wheel, 1000 g load, ASTM D3489
Thermal Properties Metric English Comments
Vicat Softening Point 50.0 °C
122 °F
Rate A; ASTM D1525
Glass Transition Temp, Tg -55.0 °C
-67.0 °F
DMA