Flexural Modulus 35.0 GPa
5080 ksi
Lehmann & Voss LUVOCOM® 1115/XCF/40 PEK, with carbon fiber
Applications: High-strength and high-stiff parts; low coefficient of expansion.Dynamic stressed parts at high movement velocity.Chemical and hydrolysis resistance parts, non flammable.Electrically c..
Flexural Modulus 35.0 GPa
5080 ksi
Saint-Gobain Quartzel® Fiber/Epoxy Resin Unidirectional Composite
Quartzel® fiber is produced from quartz crystal that is ground, purified, fiberized by a fusion process. It is homogeneous, non-porous, continuous, amorphous, ultra pure silica glass. It is of..
Flexural Modulus 35.0 GPa
5080 ksi
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, E-glass UD fabric 315 g/m2
Information provided by HexCel
Flexural Modulus 35.0 GPa
5080 ksi
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, E-glass UD fabric 430 g/m2
Information provided by HexCel
Flexural Modulus 35.0 GPa
5080 ksi
Hexcel® HexPly® ES70 120°C Curing Epoxy Matrix, Hybrid carbon/Aramid fabric 245 g/m2
Information provided by HexCel
Flexural Modulus 35.0 GPa
5080 ksi
transverse; ISO 178
Bond Laminates TEPEX® dynalite 408-C200(2)-FG290(4)/45% Carbon – Filament Glass – TPU Consolidated Composite Laminate