Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.355 GPa | 51.5 ksi | ASTM D790 |
ExxonMobil Iotek® 8030 Sodium Ionomer Molding/Extrusion Resin
(discontinued **) Data provided by the manufacturer, Exxon Chemical.Excellent abrasion resistance, impact strength, hardness, and tensile strength. Iotek ionomers provide superb low temperature impact strength when .. |