ExxonMobil Iotek® 8030 Sodium Ionomer Molding/Extrusion Resin  (discontinued **)

Category Polymer , Thermoplastic , Ionomer , Ionomer, Molded
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil Iotek® 8030 Sodium Ionomer Molding/Extrusion Resin  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by the manufacturer, Exxon Chemical.Excellent abrasion resistance, impact strength, hardness, and tensile strength. Iotek ionomers provide superb low temperature impact strength when blended with other polymers.Applications: Golf ball covers; Injection molded articles; Shoe heel counters/stiffeners; Bowling pins; Auto rub strips.
Physical Properties Metric English Comments
Density 0.956 g/cc
0.0345 lb/in³
Exxon Method
Melt Flow 2.8 g/10 min
2.8 g/10 min
Exxon Method
Mechanical Properties Metric English Comments
Hardness, Shore D 60
60
ASTM D2240
Tensile Strength, Ultimate 32.0 MPa
4640 psi
ASTM D638
Elongation at Break 410 %
410 %
ASTM D638
Flexural Modulus 0.355 GPa
51.5 ksi
ASTM D790
Tensile Impact Strength 500 kJ/m²
238 ft-lb/in²
23°C; ASTM D-1822
Thermal Properties Metric English Comments
Melting Point 87.0 °C
189 °F
Exxon Method
Vicat Softening Point 55.0 °C
131 °F
Rate B; ASTM D-1525