Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.10 GPa | 595 ksi | |
Plastcom SLOVASTER® B GF 6 FRL 4 PBT, 6% glass fibre, flame retarder FeaturesPBT with the content of 6 % chemically bound glass fibre and with the flame retardant on the basis of bromine hydrocarbons. Anisotropy of shrinkage enables the injection moulding of round, c.. |
|||
Flexural Modulus | 4.10 GPa @Temperature 23.0 °C |
595 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYblend 85 M10 PC/ABS-Blend Information provided by Polykemi AB |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ISO 178 |
Panjin Zhongrun Chemerize 085P Low Viscosity CoPEEK Information provided by Bieglo Gmbh. |
|||
Flexural Modulus | 4.10 GPa @Temperature 23.0 °C |
595 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH GF1020 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | 1.3 mm/min; ASTM D790 |
PolyOne Edgetek® X TR2-30TA/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ISO 178 |
Nilit FRIANYL A63 AL40 Nylon 6.6 for injection molding, 40% aluminum filled Nylon 6.6 for injection moldingInformation provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ASTM D790 |
Gharda Chemicals G-PAEKâ„¢ 1200G Ultra High Performance PEK Polymer Product Details: Ultra High Performance Thermoplastic (Poly Aryl Ether Ketone) material, virgin semi-crystalline granules suitable for injection molding, easy flow, Beige in colorApplication Areas:.. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | 2 mm/min; ISO 178 |
Inno-Comp INNOPOL® CS 1-3140 40% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-3140 is a 40% talc-filled polypropylene homopolymer compound. This grade is available in natural and custom colored form.INNOPOL® CS 1-3140 is recommended especially for producin.. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | conditioned, 2 mm/min; ISO 178-A |
Lanxess Durethan® DP 2131/20 H3.0 000000 Nylon 6, 20% Glass Fiber PA 6, 20% glass fiber, injection molding, heat-ageing stabilized, weather stabilized, improved surface finishInformation provided by LANXESS. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP JF002 PES (Europe-Africa-Middle East) LNP* Thermocomp* JF002 is a compound based on Polyethersulfone resin containing Glass Fiber. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GTX GTX8410W PPE+PA High flow, 10% Glass Reinforced PPE+PA. Typically used in Automotive connectors. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | Tangent |
Schmelzer Industries Pearlveil 110-7 Fiberglass Veil Economical alternative for flat or shallow applications. Suitable for hand lay-up, pre-form molding, press molding, vacuum molding, and injection molding. Data provided by the manufacturer, Schmelz.. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ASTM D790 |
Tipco Tipcofil® AG 200 - 10% Glass Fiber Reinforced Nylon-6 Compound, with High Heat Stability 10% Glass Reinforced Nylon-6 CompoundApplications: General PurposeProcessing: Injection MoldingInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ISO 178-93 |
Wellman Wellamid® GFT15N050-BK2 15% Glass Fiber Toughened Nylon 66 Description: Glass Fiber Toughened Nylon 66Information provided by Wellman. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ISO 178 |
Polyram RamOfin PPH316G4 Polypropylene, 20% Glass Fiber 20% Glass fiber reinforced, high heat stabilized polypropylene for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ISO 178 |
Ecomass® 2150TU96 Tungsten Powder Filled Polyamide (PA6/6), Injection Molding Grade Tungsten Powder Filled Polyamide (PA6/6), Good Toughness, Product Form - PelletsProcessing Method: Injection MoldingNontoxic alternative to Lead, weighting, balancing and radiation shielding applic.. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide BS6 PA6, 30% Glass Bead Filled, Injection Molded Staramide BS6 is a 30% Glass Bead Reinforced, Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | 2 mm/min; ISO 178 |
Eurostar Starpylen MF004S PP, 20% Glass Fiber Filled, Injection Molded Starpylen MF004S is a 20% Glass Fiber Reinforced Polypropylene Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ASTM D790 |
Adell BJ-14 Nylon 6, 20% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ASTM D790 |
Adell BJ-34 Nylon 6, 20% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ASTM D790 |
Adell BT-13 Nylon 6, 15% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 511 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.10% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ASTM D790 |
Ashley Polymers Ashlene® 63M Nylon 66, Mineral Filled A mineral filled Nylon 66 providing superior stiffness and dimensional stability.Data provided by the manufacturer |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 462 Glass Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.15% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ASTM D790 |
A. Schulman ComAlloy Lubrilon® 631 Nylon 6/6, Graphite/Molybdenum Disulfide Filled Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | 2 mm/min, 64mm span; ISO 178 |
SABIC Innovative Plastics SABIC PPCOMPOUND 19T1030 PP SABIC® PPcompound 19T1030 is a general purpose, talc filled, heat stabilized homopolymer polypropylene compound. This compound exhibits high flow and is suitable for injection molding applications... |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | 2 mm/min, 64mm span; ISO 178 |
SABIC Innovative Plastics SABIC STAMAX 20YM240 PP SABIC® STAMAX 20YM240 is a 20% long glass fiber reinforced polypropylene. The glass fibers are chemically coupled to the PP matrix, resulting in high stiffness and strength. The IMDS is 62455287. |
|||
Flexural Modulus | 4.10 GPa @Temperature 23.0 °C |
595 ksi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 380P Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, medium flow, FDA food contact compli.. |