Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.10 GPa | 595 ksi | |
Plastcom SLOVASTER® B GF 6 FRL 4 PBT, 6% glass fibre, flame retarder FeaturesPBT with the content of 6 % chemically bound glass fibre and with the flame retardant on the basis of bromine hydrocarbons. Anisotropy of shrinkage enables the injection moulding of round, c.. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ISO 178 |
Panjin Zhongrun Chemerize 085P Low Viscosity CoPEEK Information provided by Bieglo Gmbh. |
|||
Flexural Modulus | 4.10 GPa @Temperature 23.0 °C |
595 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYfill PPH GF2020 PD2 Polypropylene Homopolymer, Glass Fibre-Reinforced, Chemically Coupled Information provided by Polykemi AB |
|||
Flexural Modulus | 4.10 GPa @Temperature 23.0 °C |
595 ksi @Temperature 73.4 °F |
ISO 178 |
PolyOne Bergamid™ B70 G/GK30 TM-Y UV NC Polyamide 6 (Nylon 6) Information provided by PolyOne |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | 1.3 mm/min; ASTM D790 |
PolyOne Edgetek® X TR2-30TA/000 NATURAL Copolyester The Edgetek™ engineering thermoplastics compounds made with Eastman Tritan™ copolyester offer a wide range of performance and properties with the addition of reinforcing additives. By utilizing Ea.. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ISO 178 |
Victrex® PEEK 600G Polyetheretherketone
(discontinued **) Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ASTM D790 |
North Wood Plastics HDPE with 60% Wood Fiber Data provided by North Wood Plastics, Inc. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | 2 mm/min; ISO 178 |
Inno-Comp INNOPOL® CS 1-4140 BAP 40% Talc-Filled Polypropylene Homopolymer INNOPOL® CS 1-4140 B AP is a 40% talc-filled polypropylene homopolymer compound /PP-H TD40 (ISO 1043)/.INNOPOL® CS 1-4140 B AP is recommended especially for producing products, where high stif.. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | conditioned, 2 mm/min; ISO 178-A |
Lanxess Durethan® DP 2131/20 H3.0 000000 Nylon 6, 20% Glass Fiber PA 6, 20% glass fiber, injection molding, heat-ageing stabilized, weather stabilized, improved surface finishInformation provided by LANXESS. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ISO 178 |
Solvay TECHNYL® A 548B V15 PA66, 15% glass fiber, DRY Description: TECHNYL® A 548B V15 is a copolyamide 6.6/6, reinforced with 15% of glass fiber, heat stabilized, impact modified, for blow molding. This product is available in black color.Benefits:.. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ASTM D790 |
Solvay TECHNYL® C 246SI V11 PA6, 11% glass filled, DRY Description: Polyamide 6, reinforced with 11% of glass fiber, with high impact resistance, for injection molding.Available in: Asia PacificProduct Applications: TECHNYL® C 246SI V11 has good mech.. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP LUBRICOMP UX06002 PPA (Europe-Africa-Middle East) LNP* LUBRICOMP* UX06002 is a compound based on Polyphthalamide resin containing Aramide Fiber, PTFE. Added features include: Easy Molding, Internally Lubricated, Heat Stabilized. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ASTM D790 |
Techmer ES HiFill® PEEK 150 Availability: North AmericaForms: PelletsFeatures: Low ViscosityInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ASTM D790 |
Techmer ES HiFill® PEEK 450 BK Availability: North AmericaForms: PelletsFeatures: High ViscosityAppearance: BlackInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP JF002 PES (Europe-Africa-Middle East) LNP* Thermocomp* JF002 is a compound based on Polyethersulfone resin containing Glass Fiber. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP DF0029ER PC LNP* Thermocomp* DF0029ER is a compound based on Polycarbonate resin containing 10% Glass Fiber. Added features of this material include: Easy Molding, Mold Release, Flame Retardant. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp MF004S PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MF004S is a compound based on Polypropylene resin, containing Glass Fiber. Added features include; Chemically Coupled.This data was supplied by SABIC-IP for the Europe-Africa-Middle.. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ISO 178 |
Polyram RamOfin PPH316G4 Polypropylene, 20% Glass Fiber 20% Glass fiber reinforced, high heat stabilized polypropylene for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | Extruded Rod; ISO 178 |
Westlake Plastics MediPEEK IM Polyetheretherketone for Medical Applications MediPEEK-IM is a high performance semi-crystalline thermoplastic designed for long term body contact as an implantable material. It is USP Class VI and compliant to ASTM F2026. It has excellent st.. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ASTM-D790 |
Polyram PlusTek PB351I6 Nylon 6, 30% Glass Fiber and Mineral 30% glass fiber and mineral reinforced polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ISO 178 |
Polyram Polytron P20B03 Polypropylene, 20% Long Glass Fiber A chemically coupled 20% long glass fibers reinforced black polypropylene, heat stabilized for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ISO 178 |
Polyram RamLloy PFS302G14 ASA/PBT Alloy, 14% Glass Fiber 14% Glass fiber reinforced ASA/PBT alloy for injection molding applications.Information provided by Polyram. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ASTM D790 |
Adell BT-13 Nylon 6, 15% Glass Reinforced; Impact Modified Data provided by Adell Plastics, Inc. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ASTM D790 |
Chem Polymer Chemlon 214 G Nylon 6, 14% Glass Fiber Reinforced A 14% glass fiber reinforced nylon 6 offering improved creep resistance, stiffness, tensile and dimensional stability over unmodified nylon 6 materials.Data provided by the manufacturer, Chem Polyme.. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 511 Polycarbonate, Glass Reinforced, UL Data provided by the manufacturer, ComAlloy International Company.10% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ASTM D790 |
A. Schulman ComAlloy Lubrilon® 511 Polycarbonate, Glass Fiber/PTFE, UL Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ASTM Test |
BASF Ultramid® B3M6 30% Mineral Filled PA6 (Dry) Ultramid B3M6 is a 30% mineral reinforced injection molding PA6 grade for industrial items requiring high impact strength and very high dimensional stability, excellent laser markability. |
|||
Flexural Modulus | 4.10 GPa | 595 ksi | ASTM D790 |
A. Schulman ComAlloy Lubrilon® 631 Nylon 6/6, Graphite/Molybdenum Disulfide Filled Data provided by the manufacturer, ComAlloy International Company. High performance and excellent lubricity with minimal surface wear.The ComAlloy product line has been integrated into the A Schulma.. |
|||
Flexural Modulus | 4.10 GPa @Temperature 23.0 °C |
595 ksi @Temperature 73.4 °F |
ISO 178 |
Victrex® PEEK 380P Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, coarse powder for extrusion compounding, medium flow, FDA food contact compli.. |