Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.00 - 6.30 GPa | 870 - 914 ksi | 20% Glass Laminate |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |
|||
Flexural Modulus | 6.00 - 6.30 GPa | 870 - 914 ksi | 20% Glass Laminate |
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica.. |