Polymer Property : Flexural Modulus = 6.43 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 6.20 - 6.43 GPa
899 - 933 ksi
Average value: 6.26 GPa Grade Count:4
Overview of materials for PVC, 20% Glass Fiber Reinforced
This property data is a summary of similar materials in the MatWeb database for the category "PVC, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are included. E..