Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.53 GPa | 947 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP STAT-KON DEL329E PC (Asia Pacific) LNP* Stat-kon* DEL329E is a compound based on Polycarbonate resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, .. |
|||
Flexural Modulus | 6.53 GPa | 947 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP 9X02540 PC+PET LNP* THERMOCOMP* PDX-02540 is a compound based on a PET+PC Blend containing Proprietary Filler. Flame Retardant. |