Mechanical Properties Metric English Comments
Flexural Modulus 6.53 GPa
947 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP STAT-KON DEL329E PC (Asia Pacific)
LNP* Stat-kon* DEL329E is a compound based on Polycarbonate resin containing PTFE, Flame Retardant, Carbon Fiber. Added features of this material include: Electrically Conductive, Flame Retardant, ..
Flexural Modulus 6.53 GPa
947 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP THERMOCOMP 9X02540 PC+PET
LNP* THERMOCOMP* PDX-02540 is a compound based on a PET+PC Blend containing Proprietary Filler. Flame Retardant.