Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.55 GPa | 950 ksi | Tangent; ASTM D790 |
RheTech Products F56-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Consumer goodsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
PolyOne Maxxam™ PPC-40G Black Polypropylene Copolymer (PP Copolymer) PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium car.. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
Polymer Resources PCSF-FR G30 Polycarbonate, 30% Glass Reinforced Structural Foam Grade Process: Foam MoldingNotes: All physical, mechanical and thermal testing conducted on 1/8-inch thick, un-pigmented, test samples. Foam grades tested with foamed parts with a 10% weight reduction rel.. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
Quadrant EPP Semitron® ESd 490HR Static dissipative PEEK for use in test fixtures. Non-sloughing and low moisture absorption. (ASTM Product Data Sheet) |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
PolyOne Edgetek® AS-30GF/000 Acrylonitrile Butadiene Styrene (ABS), Glass Filled
(discontinued **) Description/Features:Glass Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
Global MPP-140-C 40% Mica Reinforced Polypropylene Information provided by Global Polymers Corporation. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Asia Pacific) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE (Europe-Africa-Middle East) 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Europe-Africa-Middle East regio.. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
Techmer ES HiFill FR® PA6/6 GF25 FR BK 25% Glass Filled (Conditioned) Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber, 25% Filler by WeightAdditive: Heat Stabilizer and LubricantFeatures: Flame Retardant, Heat Stabilized and LubricatedAppear.. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
Techmer ES HiFill® POM CO GF20 CC 20% Glass Filled Availability: North AmericaForms: PelletsFiller/Reinforcement: Glass Fiber Reinforced, 20% Filler by WeightFeatures: Copolymer and Chemically CoupledInformation provided by TP Composites, Inc. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | 1.3 mm/min, 50 mm span; ASTM D 790 |
SABIC Innovative Plastics Ultem ATX152R PEI+PCE 20% Glass fiber filled, high flow Polyetherimide blend with internal mold release. ECO Conforming, UL94 V0 and 5VA listing.This data was supplied by SABIC-IP for the Americas region. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF20H 20% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF20H 20% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
A. Schulman SCHULAMID® 66 GF20H 20% Glass Fiber Reinforced, Heat Stabilized Nylon 66 Information provided by A. Schulman. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
Aaron Industries AAROPRENE® G/MFN 6002 Glass and Mineral Filled Nylon 6 AAROPRENE® GFN &G/MFN 6000 Series Reinforced CompoundsColor may be specified. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
Chase Plastics CP Pryme® NN133GTL (DAM) Nylon 66, 33% Glass Fiber Reinforced, Toughened, Internally Lubricated Information provided by Chase Plastics. |
|||
Flexural Modulus | 6.55 GPa | 950 ksi | ASTM D790 |
Chase Plastics CP Pryme® PC330R Polycarbonate, 30% Glass Fiber Reinforced, Recycled Content Features: Good mold releaseRecycled contentForm: PelletsInformation provided by Chase Plastics. |