Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Maxxam™ PPC-40G Black Polypropylene Copolymer (PP Copolymer)

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer PolyOne Corporation
Trade Name Maxxam™
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Maxxam™ PPC-40G Black Polypropylene Copolymer (PP Copolymer).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PolyOne's Maxxam™ family of polypropylene- and polyethylene-based products covers a wide range of applications, markets and performance requirements. Standard grades are compounded with calcium carbonate, glass and talc to provide a desired balance of properties including stiffness, durability, impact resistance and heat resistance. Custom grades are available with features such as UV stabilizers, heat stabilizers, custom color, high impact, etc.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm
0.0020 - 0.0050 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Yield 65.5 MPa
9500 psi
Type I, 51 mm/min; ASTM D638
Elongation at Break 5.0 %
5.0 %
Type I, 51 mm/min; ASTM D638
Flexural Strength 88.3 MPa
12800 psi
ASTM D790
Flexural Modulus 6.55 GPa
950 ksi
ASTM D790
Izod Impact, Notched 0.530 J/cm

@Thickness 3.18 mm,
Temperature 23.0 °C
0.993 ft-lb/in

@Thickness 0.125 in,
Temperature 73.4 °F
Injection Molded; ASTM D256A
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 156 °C

@Thickness 3.18 mm
313 °F

@Thickness 0.125 in
Annealed; ASTM D648
Processing Properties Metric English Comments
Mold Temperature 16.0 - 50.0 °C
60.8 - 122 °F
Descriptive Properties Value Comments
Additive Impact Modifier
Appearance Black
Features Copolymer
General Purpose
Impact Modified
Filler / Reinforcement Glass Fiber Reinforcement
Unspecified FillerReinfor., 40% Filler by Weight
Forms Pellets
Generic Material PP Copolymer
Generic Name Polypropylene Copolymer (PP Copolymer)
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Applications
Construction Applications
Consumer Applications
General Purpose
Industrial Applications
Users viewing this material also viewed the following: