Polymer Property : Flexural Modulus = 6.82 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 6.82 GPa
989 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRILOY RF206 PA 66 (Europe-Africa-Middle East)
LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Flexural Modulus 6.82 GPa
989 ksi
ASTM D 790
SABIC Innovative Plastics LNP Lubriloy RF206H PA 66
LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Lubricant, Lubricants. Added features of this material include: Internally Lubricated.This data was su..
Flexural Modulus 6.82 GPa
989 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRILOY RF206H PA 66 (Asia Pacific)
LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated.
Flexural Modulus 6.82 GPa
989 ksi
ASTM D790
SABIC Innovative Plastics LNP LUBRILOY RF206XXH PA 66
LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare
Flexural Modulus 6.82 GPa
989 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOTUF PF006I PA 6
LNP THERMOTUF* PF006I is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: High Impact.