Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 6.82 GPa | 989 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY RF206 PA 66 (Europe-Africa-Middle East) LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 6.82 GPa | 989 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Lubriloy RF206H PA 66 LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Proprietary Lubricant, Lubricants. Added features of this material include: Internally Lubricated.This data was su.. |
|||
Flexural Modulus | 6.82 GPa | 989 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY RF206H PA 66 (Asia Pacific) LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing Glass Fiber, Lubricants, Proprietary Lubricant. Added features of this material include: Internally Lubricated. |
|||
Flexural Modulus | 6.82 GPa | 989 ksi | ASTM D790 |
SABIC Innovative Plastics LNP LUBRILOY RF206XXH PA 66 LNP LUBRILOY* RF206H is a compound based on Nylon 66 resin containing 30% Glass Fiber, Proprietary Lubricant. Added features of this material include: Wear Resistant, Healthcare |
|||
Flexural Modulus | 6.82 GPa | 989 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOTUF PF006I PA 6 LNP THERMOTUF* PF006I is a compound based on Nylon 6 resin containing Glass Fiber. Added features of this material include: High Impact. |