Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.169 GPa | 604.7 ksi | ISO 178 |
Ecomass® 4301TU74 Tungsten Filled Polyphthalamide Nontoxic alternative to Lead (Pb), weighting, balancing and radiation shielding applicationsTungsten Powder Filled Polyphthalamide (PPA)Very Good ToughnessInformation provided by Technical Polymers |