Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 4.40 GPa | 638 ksi | STN EN ISO 178 |
Plastcom PLASTAMID® 6 GF 15 PA6 reinforced with glass fiber PA 6 for injection molding, reinforced with 15% glass fiber. Application: applied in automotive, electrical, engineering and consumer-goods industry, eg.: grips for electro tools, hobby tools, gears.. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics Cycoloy® CM6240 PC+ABS (Asia Pacific) CYCOLOY CM6240 resin is a flame retardant PC/ABS blend featuring balanced properties of high modulus, good flow and ductility. It is of Br- & Cl-free flame retardant systems intended to meet thin wa.. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® XCM851 PC+ABS High heat PC/ABS blend offering high modulus / low CTE and good practical impact |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics Cycoloy® XCM851 PC+ABS (Europe-Africa-Middle East) High heat PC/ABS blend offering high modulus / low CTE and good practical impactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | |
Plastcom SLOVAMID 6 GF 15 HI PA6, 15% glass fibre, improved strength FeaturesPA 6 for injection moulding, chemically strengthened with 15% glass fibre. Application: impacted mouldings and mouldings with high strength applied in automotive, electrical, engineering and.. |
|||
Flexural Modulus | 4.40 GPa @Temperature 23.0 °C |
638 ksi @Temperature 73.4 °F |
ISO 178 |
Polykemi AB POLYshine PBT D201 T20 PBT, Reinforced Information provided by Polykemi AB |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | ASTM D790 |
PolyOne Stat-Tech™ PF-05CF/000 EM FR Flame Retardant Polysulfone - 5% Carbon Fiber
(discontinued **) Data provided by PolyOne. |
|||
Flexural Modulus | 4.40 GPa @Temperature 23.0 °C |
638 ksi @Temperature 73.4 °F |
DAM; ISO 178 |
DuPont Performance Polymers Zytel® 80G14AHS BK099 Nylon 66
(Unverified Data**) Zytel® 80G14AHS BK099 is a 14% glass fiber reinforced, toughened, high flow, heat stabilized, black polyamide 66 resin. It offers outstanding performance in injection molding applications.Informati.. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Asia Pacific) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly LNP* THERMOCOMP* KF002L is a compound based on Acetal Homopolymer resin containing 10% Glass Fiber. Added features of this material include: Low Extractible. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | ISO 178 |
SABIC Innovative Plastics LNP THERMOCOMP KF002L Acetal Homopoly (Asia Pacific) LNP* Thermocomp* KF002L is a compound based on Acetal Homopolymer resin containing Glass Fiber. Added features of this material include: Low Extractible. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | 2mm/min; ISO 178 |
Teijin Panlite® G-3120PH For Cameras, Glass Fiber Reinforced Polycarbonate Resin Reinforced with 30 % of special GF and improved appearance grade.Applications:Precision machinery, electric and electronic components that need dimensional accuracy and good appearance.Information p.. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp MH0255A PP (Europe-Africa-Middle East) LNP* THERMOCOMP* MH0255A is a compound based on Polypropylene resin containing Proprietary Filler(s). Added features include; High Specific Gravity.This data was supplied by SABIC-IP for the Europe-.. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics LNP Thermocomp RB008 PA 66 (Europe-Africa-Middle East) LNP* THERMOCOMP* RB008 is a compound based on PA 66 resin containing Glass Bead.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | ISO 178 |
Borealis GB205U Polypropylene Compound, Glass Fiber Reinforced GB205U is a 20% chemically coupled glass fiber reinforced polypropylene compound intended for injection molding. The product is available in natural but other colors can be provided on request. Thi.. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | ASTM D790 |
Tipco Tipcolene® FPT 40 NEX - 40% Talc Reinforced Polypropylene Homopolymer, Low MFI 40% Talc Reinforced PP HomopolymerApplications: Sheets, Pipes, ProfilesProcessing: ExtrusionInformation provided by the Manufacturer, Tipco Industries Ltd.,
India. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | ISO 178 |
Polyram RamSter PF302G3 PBT, 15% Glass Fiber, UV Stabilized 15% Glass fiber reinforced, UV stabilized PBT for injection molding application.Information provided by Polyram. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | At 2 mm/min; ISO 178 |
Borealis Xmod™ K65G2 20% Glass Fiber Reinforced Polypropylene Compound Xmod K65G2 is a 20% glass fiber reinforced grade intended for injection molding. Xmod K65G2 has been developed especially for the car industry, to be used UTB parts. Xmod K65G2 offers good balance.. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | ISO 178 |
Hexcel® HexPly® 6376 175°C Curing Epoxy Matrix HexPly® 6376 is a high performance tough matrix formulated for the fabrication of primary aircraft structures. It offers high impact resistance and damage tolerance for a wide range of high tempera.. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | DAM; ISO 178 |
DuPont Performance Polymers Minlon® 12TA BKB124 Nylon 66
(Unverified Data**) 32% Mineral Reinforced Toughened Polyamide 66 Minlon 12TA BKB124 is a 32% mineral reinforced toughened heat stabilized black polyamide 66 resin for injection molding.Information provided by DuPont P.. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide PFB42U PA6, Glass Fiber/Bead Filled, Injection Molded Starflam PFB42U is an UV Stabilized, Glass Bead and Glass Fiber Reinforced Polyamide 6 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | 2 mm/min; ISO 178 |
Eurostar Starpylen HZ 80E7 HDPE, Injection Molding Starpylen HZ 80E7 is a High Specific Gravity Polypropylene, Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | 2 mm/min; ISO 178 |
Eurostar Staramide RB008 PA66, 40% Glass Bead Filled, Injection Molded Staramide RB008 is a 40% Glass Bead Reinforced Polyamide 66 Injection Molding ResinInformation provided by Eurostar. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | ISO 178 |
Azdel Plus R300-B01 30% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R300-B01 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a polypropylene resin matrix. This composite material features high flow pr.. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | ISO 178 |
Azdel Plus R300B01N 30% Continuous Random Fiber Mat / PP Resin Matrix AZDEL® R300B01N is a random oriented needled continuous glass fiber mat material. This polypropylene composite material features high properties and a homogeneous fiber distribution. This materia.. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | ASTM D790 |
Beijing Chemical Industry KAIFA® M109-G20 MPPO Resin 20% glass fiber reinforcedInformation provided by Beijing Chemical Industry Research Institute (Group) |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | ASTM D790 |
A. Schulman ComAlloy Hiloy® 422 Heavy Mineral Reinforced, PBT Alloy Data provided by the manufacturer, ComAlloy International Company.40% Heavy Mineral Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | 2 [mm/min]; ISO 178 |
Akro-Plastic Akromid® A3 GF 10 (2852) PA 6.6 Dry, 10% Glass Filled AKROMID® A (Polyamide 6.6) is an engineering compound, characterized by high mechanical strength, stiffness and thermal resistance. Furthermore, this polyamide offers high toughness at low temperat.. |
|||
Flexural Modulus | 4.40 GPa | 638 ksi | 2 mm/min; ISO 178 |
Sax Polymers SAXALEN PPH304G25 Polypropylene Homopolymer, 25% Glass Filled SAXALEN PPH304G25 is a 25% glass filled Polypropylene - Homopolymer intended for injection molding. This compound is characterized by high stiffness good impact resistance und reduced creep under lo.. |