Hexcel® HexPly® 6376 175°C Curing Epoxy Matrix

Category Polymer , Thermoset , Epoxy , Epoxy Cure Resin
Manufacturer Hexcel
Trade Name HexPly®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Hexcel® HexPly® 6376 175°C Curing Epoxy Matrix.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
HexPly® 6376 is a high performance tough matrix formulated for the fabrication of primary aircraft structures. It offers high impact resistance and damage tolerance for a wide range of high temperature applications.Information provided by HexCel
Physical Properties Metric English Comments
Density 1.31 g/cc
0.0473 lb/in³
Cured
Mechanical Properties Metric English Comments
Tensile Strength, Yield 105 MPa
15200 psi
ISO R527 Type 1
Elongation at Yield 3.1 %
3.1 %
ISO R527 Type 1
Tensile Modulus 3.60 GPa
522 ksi
ISO R527 Type 1
Flexural Yield Strength 144 MPa
20900 psi
ISO 178
Flexural Modulus 4.40 GPa
638 ksi
ISO 178
Toughness 432 J
319 ft-lb
Per square meter
Processing Properties Metric English Comments
Shelf Life >= 6.00 Month

@Temperature -18.0 °C
>= 6.00 Month

@Temperature -0.400 °F