Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 46.5 GPa | 6740 ksi | ASTM D790 |
Quantum Composites LYTEX® 4197 55% Carbon Fiber Reinforced Epoxy SMC LYTEX 4197 is an epoxy high performance, 3K tow carbon fiber (PAN) reinforced engineered structural composite (ESC) molding compound designed for military and aerospace structural applications requi.. |