Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Quantum Composites LYTEX® 4197 55% Carbon Fiber Reinforced Epoxy SMC

Category Polymer , Thermoset , Composite SMC , Epoxy , Epoxy/Carbon Fiber Composite
Manufacturer Quantum Composites
Trade Name Lytex®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Quantum Composites LYTEX® 4197 55% Carbon Fiber Reinforced Epoxy SMC.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LYTEX 4197 is an epoxy high performance, 3K tow carbon fiber (PAN) reinforced engineered structural composite (ESC) molding compound designed for military and aerospace structural applications requiring excellent mechanical properties, retention of properties at elevated temperatures, good chemical resistance and low density.Form = SheetColor = BlackGlass Fiber Content = 55%Information provided by Quantum Composites.
Physical Properties Metric English Comments
Specific Gravity 1.45 g/cc
1.45 g/cc
ASTM D792
Linear Mold Shrinkage 0.00 cm/cm
0.00 in/in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength 275 MPa
39900 psi
ASTM D638
Tensile Modulus 62.0 GPa
8990 ksi
ASTM D638
Flexural Strength 689 MPa
99900 psi
ASTM D790
Flexural Modulus 46.5 GPa
6740 ksi
ASTM D790
Izod Impact, Notched 15.0 J/cm
28.1 ft-lb/in
ASTM D256
Processing Properties Metric English Comments
Processing Temperature 129 - 166 °C
265 - 330 °F
Mold Temperature
Cure Time 5.00 - 10.0 min
0.0833 - 0.167 hour
Shelf Life 6.00 Month

@Temperature -17.8 °C
6.00 Month

@Temperature 0.000 °F
Descriptive Properties Value Comments
Fiber Length (in) 2
Carbon
Users viewing this material also viewed the following: