Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.16 GPa | 1040 ksi | ASTM D790 |
Samyang Tribit® 1550GN30 PBT Alloy, Reinforced Flame Retardancy Crystallization is fast, formability is excellent and thermal resistance, chemical resistance, electrical properties and abrasion resistance are excellent.1550GN30 is a reinforced, flame retardant (.. |
|||
Flexural Modulus | 7.16 GPa | 1040 ksi | ASTM Test |
BASF Ultramid® 8267G HS BK-106A 15/25% Glass/Mineral Filled PA6 (Dry) Ultramid 8267G HS BK-106A is a heat stabilized, weather resistant, 40% mineral and glass fiber reinforced PA6 injection molding compound with improved UV resistance and sink mark resistance. The co.. |
|||
Flexural Modulus | 7.16 GPa | 1040 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP STAT-KON QE002S PA6.10 LNP* STAT-KON* QE002S is a compound based on Nylon 6/10 containing 10% carbon Fiber. Added features of this material include: Heat Stabilized, Electrically Conductive. |