Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 7.17 GPa | 1040 ksi | ISO 178 |
Ravago Manufacturing Americas Hylon® N1240MHL BK Nylon 6/6 Available in North America Filler: Mineral, 40% Filler by WeightAdditive: Heat Stabilizer and Lubricant Features: Lubricated, Low Warpage and Heat StabilizedRoHS CompliantForm: Pellets Processing .. |
|||
Flexural Modulus | 7.17 GPa @Temperature 100 °C |
1040 ksi @Temperature 212 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)
(Unverified Data**) Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include .. |
|||
Flexural Modulus | 7.17 GPa | 1040 ksi | |
Malvern Minerals Epoxy with 50% Novacite® Daper Quartz Filler Novacite® quartz silica has closely controlled sizing that is used extensively in the coatings field. Novacite® has broad acceptance as silica in special purpose, product finishes OEM, automo.. |
|||
Flexural Modulus | 7.17 GPa | 1040 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL PX5558 PPE+PS 30% glass reinforced, high flow PPO. |
|||
Flexural Modulus | 7.17 GPa @Temperature 100 °C |
1040 ksi @Temperature 212 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry) Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp.. |
|||
Flexural Modulus | 7.17 GPa | 1040 ksi | 2 mm/min; ISO 178 |
SABIC Innovative Plastics ULTEM SF2260 PEI Blend (Asia Pacific) High flow Ultem for thin wall application |
|||
Flexural Modulus | 7.17 GPa | 1040 ksi | ASTM D 790 |
SABIC Innovative Plastics LNP Thermocomp RFZ349 PA 66 (Asia Pacific) LNP* Thermocomp* RFZ349 is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. Added features of this material include: Flame Retardant.This data was supplied by SABIC-IP for t.. |
|||
Flexural Modulus | 7.17 GPa | 1040 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RFZ349XC PA 66 LNP THERMOCOMP* RFZ349XC is a compound based on Nylon 66 resin containing 20% Glass Fiber, 15% Milled Glass. Added features of this material include: Flame Retardant. |
|||
Flexural Modulus | 7.17 GPa | 1040 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP RFZ349XC PA 66 (Asia Pacific) LNP* THERMOCOMP* RFZ349XC is a compound based on Nylon 66 resin containing Glass Fiber, Milled Glass. Added features of this material include: Flame Retardant. |
|||
Flexural Modulus | 7.17 GPa | 1040 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL EM7430 PPE+PS 30% glass reinforced, high flow PPO. Automotive. Energy management material. |
|||
Flexural Modulus | 7.17 GPa | 1040 ksi | 2.6 mm/min, 100 mm span; ASTM D790 |
SABIC Innovative Plastics NORYL GFN3 PPE+PS PPE+PS blend. 30% Glass reinforced. NSF 61 listing in several colors (restrictions apply). FDA compliance (restrictions apply). Low water absorption. Hydrolytic stability. Dimensional stability. Sui.. |
|||
Flexural Modulus | 7.17 GPa | 1040 ksi | ASTM D790 |
Teknor Apex Sinpolene GPP1640 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Additive: Glass Fiber Reinforcement, 40% Filler by Weight Features: Good Dimensional Stability; High Heat Resistance; .. |
|||
Flexural Modulus | 7.17 GPa | 1040 ksi | (102 mm Span) 3mm/min; ASTM D790 |
LNP ULTEM® SMU5806 Polyetherimide, 8% Carbon Fiber Reinforcement
(discontinued **) Features: Low ShrinkageForms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still.. |
|||
Flexural Modulus | 7.17 GPa @Temperature 100 °C |
1040 ksi @Temperature 212 °F |
ISO 178 |
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp.. |