Polymer Property : Flexural Modulus = 7.20 GPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.20 - 7.20 GPa

@Temperature -40.0 - 80.0 °C
174 - 1040 ksi

@Temperature -40.0 - 176 °F
Average value: 4.55 GPa Grade Count:1
Overview of materials for Nylon 6, 20% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 20% Mineral Filled". Specific grades with primary filler content between 15% and 24% are includ..