Mechanical Properties Metric English Comments
Flexural Modulus 7.26 GPa
1050 ksi
2 mm/min; ISO 178
SABIC Innovative Plastics LNP LUBRICOMP RFN14 PA 66
LNP* LUBRICOMP* RFN14 is a compound based on Nylon 66 containing 20% Glass Fiber, 5% MOS2. Added features of this grade include: Wear Resistant.
Flexural Modulus 7.26 GPa
1050 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics ULTEM SF2250 PEI Blend (Asia Pacific)
High flow Ultem for thin wall application
Flexural Modulus 7.26 GPa
1050 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics Ultem SF2250 PEI Blend (Europe-Africa-Middle East)
High flow Ultem for thin wall applicationThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Flexural Modulus 7.26 GPa
1050 ksi
Shinil Chemical SHINFLAME PC/PBT GF Flame Retardant Polymer Appliance
SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod..
Flexural Modulus 7.26 GPa
1050 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® GP-8300G MPPE, 30% Glass Filled
Information provided by Samsung Cheil Industries.
Flexural Modulus 7.26 GPa
1050 ksi
2.8 mm/min; ASTM D790
Samsung Cheil Industries Infino® GP-8300G MPPE, 30% Glass Filled
Information provided by Samsung Cheil Industries.
Flexural Modulus 7.26 GPa
1050 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics ULTEM SF2250 PEI Blend
High flow Ultem for thin wall application