Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics Ultem SF2250 PEI Blend (Europe-Africa-Middle East)

Category Polymer , Thermoplastic , Polyetherimide (PEI)
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name ULTEM
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics Ultem SF2250 PEI Blend (Europe-Africa-Middle East).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High flow Ultem for thin wall applicationThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region.
Physical Properties Metric English Comments
Specific Gravity 1.44 g/cc
1.44 g/cc
ASTM D 792
Density 1.44 g/cc
0.0520 lb/in³
ISO 1183
Water Absorption 0.20 %

@Temperature 23.0 °C,
Time 86400 sec
0.20 %

@Temperature 73.4 °F,
Time 24.0 hour
ISO 62-1
Moisture Absorption at Equilibrium 0.070 %
0.070 %
23°C / 50% RH; -
Linear Mold Shrinkage, Flow 0.0046 cm/cm
0.0046 in/in
SABIC Method
Linear Mold Shrinkage, Transverse 0.0054 cm/cm
0.0054 in/in
SABIC Method
Melt Flow 19.7 g/10 min

@Load 6.60 kg,
Temperature 337 °C
19.7 g/10 min

@Load 14.6 lb,
Temperature 639 °F
ASTM D 1238
40 g/10 min

@Load 10.0 kg,
Temperature 345 °C
40 g/10 min

@Load 22.0 lb,
Temperature 653 °F
[cm^3/10 min] Melt Volume Rate; ISO 1133
Mechanical Properties Metric English Comments
Tensile Strength at Break 157 MPa
22800 psi
5 mm/min; ISO 527
162 MPa
23500 psi
Type I, 5 mm/min; ASTM D 638
Elongation at Break 3.0 %
3.0 %
Type I, 5 mm/min; ASTM D 638
3.0 %
3.0 %
5 mm/min; ISO 527
Tensile Modulus 8.90 GPa
1290 ksi
5 mm/min; ASTM D 638
Flexural Yield Strength 197 MPa
28600 psi
1.3 mm/min, 50 mm span; ASTM D 790
Flexural Modulus 7.15 GPa
1040 ksi
2 mm/min; ISO 178
7.26 GPa
1050 ksi
1.3 mm/min, 50 mm span; ASTM D 790
Izod Impact, Notched 0.890 J/cm

@Temperature 23.0 °C
1.67 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Notched (ISO) 9.00 kJ/m²

@Temperature 23.0 °C
4.28 ft-lb/in²

@Temperature 73.4 °F
80*10*4; ISO 180/1A
Thermal Properties Metric English Comments
CTE, linear, Parallel to Flow 14.0 µm/m-°C

@Temperature -40.0 - 150 °C
7.78 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
18.0 µm/m-°C

@Temperature 23.0 - 150 °C
10.0 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
CTE, linear, Transverse to Flow 54.0 µm/m-°C

@Temperature -40.0 - 150 °C
30.0 µin/in-°F

@Temperature -40.0 - 302 °F
ASTM E 831
59.0 µm/m-°C

@Temperature 23.0 - 150 °C
32.8 µin/in-°F

@Temperature 73.4 - 302 °F
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 208 °C
406 °F
Edgew 120*10*4 sp=100mm; ISO 75/Ae
203 °C

@Thickness 3.20 mm
397 °F

@Thickness 0.126 in
unannealed; ASTM D 648
Flammability, UL94 V-0

@Thickness 1.50 mm
V-0

@Thickness 0.0591 in
UL 94 by SABIC-IP