Mechanical Properties Metric English Comments
Flexural Modulus 0.490 GPa
71.0 ksi
At 2 mm/min; ASTM D790
Borealis Borecene™ RM8342 Linear Polyethylene for Rotational Molding
Borecene RM8342 is a third generation linear medium density natural polyethylene for rotational molding. The narrow molecular weight distribution imparted through metallocene catalyst technology pro..
Flexural Modulus 0.490 GPa
71.0 ksi
At 2 mm/min; ASTM D790
Borealis Borecene™ RM8342RC Linear Polyethylene for Rotational Molding
Borecene RM8342RC is a third generation linear medium density natural polyethylene for rotational molding. Borecene RM8342RC is a special grade, which has passed many rigorous tests and can be cons..
Flexural Modulus 0.490 GPa
71.0 ksi
At 2 mm/min; ASTM D790
Borealis Borecene™ RM8343 Linear Polyethylene for Rotational Molding
Borecene RM8343 is a third generation linear medium density natural polyethylene for rotational molding. The narrow molecular weight distribution imparted through metallocene catalyst technology pro..
Flexural Modulus 0.490 GPa
71.0 ksi
At 2 mm/min; ASTM D790
Borealis Borecene™ RM8343RC Linear Polyethylene for Rotational Molding
Borecene RM8343RC is a third generation linear medium density natural polyethylene for rotational molding. Borecene RM8343RC is a special grade, which has passed many rigorous tests and can be cons..
Flexural Modulus 0.490 - 0.892 GPa
71.0 - 129 ksi
Average value: 0.632 GPa Grade Count:33
Overview of materials for Medium Density Polyethylene (MDPE), Rotational Molded
This property data is a summary of similar materials in the MatWeb database for the category "Medium Density Polyethylene (MDPE), Rotational Molded". Each property range of values reported is minimu..