Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 1.79 - 4.90 GPa
260 - 711 ksi
Average value: 2.96 GPa Grade Count:21
Overview of materials for Polypropylene, Wood Filled
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene, Wood Filled". Each property range of values reported is minimum and maximum values of app..