Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.34 - 4.96 GPa @Temperature 100 - 100 °C |
339 - 719 ksi @Temperature 212 - 212 °F |
Average value: 3.65 GPa Grade Count:2 |
Overview of materials for Polyphthalamide (PPA), 20% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 20% Glass Fiber Reinforced". Specific grades with glass content between 15% and 24% are.. |