Mechanical Properties Metric English Comments
Flexural Modulus 5.23 GPa
759 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp KF002A Acetal Homopolymer
LNP THERMOCOMP* KF002A is a compound based on Acetal Homopolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Flexural Modulus 5.23 GPa
759 ksi
ASTM D 790
SABIC Innovative Plastics LNP Thermocomp KF002A Acetal Homopolymer (Asia Pacific)
LNP THERMOCOMP* KF002A is a compound based on Acetal Homopolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Asia Pacific region.