Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

SABIC Innovative Plastics LNP Thermocomp KF002A Acetal Homopolymer

Category Polymer , Thermoplastic , Acetal (POM) , Acetal Homopolymer, Glass Fiber Reinforced
Manufacturer SABIC Innovative Plastics (GE Plastics)
Trade Name LNP THERMOCOMP
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF SABIC Innovative Plastics LNP Thermocomp KF002A Acetal Homopolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
LNP THERMOCOMP* KF002A is a compound based on Acetal Homopolymer resin containing Glass Fiber.This data was supplied by SABIC-IP for the Americas region.
Physical Properties Metric English Comments
Density 1.49 g/cc
0.0538 lb/in³
ASTM D 792
Mechanical Properties Metric English Comments
Tensile Strength at Break 85.0 MPa
12300 psi
ASTM D 638
Elongation at Break 3.1 %
3.1 %
ASTM D 638
Flexural Strength 131 MPa
19000 psi
ASTM D 790
Flexural Modulus 5.23 GPa
759 ksi
ASTM D 790
Izod Impact, Notched 0.480 J/cm

@Temperature 23.0 °C
0.899 ft-lb/in

@Temperature 73.4 °F
ASTM D 256
Izod Impact, Unnotched 4.48 J/cm

@Temperature 23.0 °C
8.39 ft-lb/in

@Temperature 73.4 °F
ASTM D 4812