Polymer Property : Flexural Modulus = 76.9 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 0.530 - 22.4 GPa
76.9 - 3250 ksi
Average value: 7.86 GPa Grade Count:164
Overview of materials for Nylon 610
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610". Each property range of values reported is minimum and maximum values of appropriate MatWeb e..
Flexural Modulus 0.530 GPa
76.9 ksi
ISO 178
Solvay TECHNYL® eXten D 458P PA6.10, Conditioned
Description: Product in development - provisional datasheet. High viscosity unfilled plasticized PA6.10 for extrusion applications providing low end part warpage.Available in: Asia Pacific, Europe, ..
Flexural Modulus 0.530 GPa
76.9 ksi
ASTM D790
3M Dyneon™ FEP 6301Z Fluorinated Ethylene Propylene Fluorothermoplastic Granules
Dyneon FEP 6301Z is offered for extrusion, injection molding and transfer molding for the wire and cable and chemical process industries. Their distinguishing features include: Excellent electrical ..
Flexural Modulus 0.530 GPa
76.9 ksi
ASTM D790
C.O.I.M. LARIPUR® LPR72D25 Special Adipate Ester Polyurethane
Description: The products of the LARIPUR® line are thermoplastic polyurethanes. These products combine the technology of thermoplastic products with the features of polyurethanes:Excellent abrasion..