Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.02 GPa | 1160 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP DX13354 PC COPOLYMER (Asia Pacific) DX13354 is 30% glass fiber reinforced, impact modified and LDS functionalized polycarbonate resin. The features include LDS function, high flow, and good ductility. |
|||
Flexural Modulus | 8.02 GPa | 1160 ksi | 1.3 mm/min, 50 mm span; ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PX85100 PA 6 LNP* THERMOCOMP* PX85100 is a compound based on Nylon 6 resin containing Proprietary Filler(s). |
|||
Flexural Modulus | 8.02 GPa | 1160 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP PX85100 PA 6 LNP* THERMOCOMP* PX85100 is a compound based on Nylon 6 resin containing Proprietary Filler(s). |