Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.22 GPa | 1190 ksi | ASTM D790 |
NYCOA ASN 27 300 KNF 30% Glass Fiber Reinforced, Heat Stabilized Nylon 6 Resin NYCOA ASN 27 300 KNF is a 30% glass fiber reinforced, heat stabilized Nylon 6 resin used for injection molding. This grade features excellent strength and stiffness, dimensional stability, and a gre.. |
|||
Flexural Modulus | 8.22 GPa | 1190 ksi | ASTM D790 |
Plenco 7300 Phenolic, Nodular, Transfer Molded
(discontinued **) Two-Stage Phenolic. PLENCO 07300 is an organic fiber reinforced phenolic molding compound offering improved mechanical strength and excellent cosmetic properties. UL recognized under component file.. |
|||
Flexural Modulus | 8.22 GPa | 1190 ksi | ISO 178 |
Azdel AZMET® CM32350 35% continuous random fiber mat / PET resin matrix AZDEL® CM20350 is a glass mat thermoplastic laminate based upon a random oriented continuous fiber mat contained within a Polyethylene Terephthalate (PET) resin matrix. This composite material fea.. |