Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 8.24 GPa | 1190 ksi | 5 mm/min; ISO 178 |
Gromax BFG30-AH00B2 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 8.24 GPa | 1190 ksi | 5 mm/min; ISO 178 |
Gromax BFG30-BN00N1 Nylon 6 30% Glass Filled (Dry) Information provided by Gromax Enterprises Corp. |
|||
Flexural Modulus | 8.24 GPa | 1190 ksi | |
Shinil Chemical SHINFLAME PBT GF Flame Retardant Polymer Lamp Housing SHINFLAME is a flame retardant (FR) compound which exhibits inherent flame retardant properties during fire. Shinil uses its patented dispersion blending technology with variety of polymers to prod.. |