Mechanical Properties Metric English Comments
Flexural Modulus 0.600 - 0.600 GPa

@Temperature 90.0 - 90.0 °C
87.0 - 87.0 ksi

@Temperature 194 - 194 °F
Average value: 0.600 GPa Grade Count:1
Overview of materials for Polybutylene Terephthalate (PBT), Flame Retardant
This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Flame Retardant". Each property range of values reported is minimum an..
Flexural Modulus 0.462 - 0.600 GPa
67.0 - 87.0 ksi
ASTM D790
Buckeye Polymers BP FLEX D0850(C) BLK Thermoplastic Polyolefin
Product Information: TPO's are a family of thermoplastic elastomers which exhibit rubber-like properties and are processable on conventional thermoplastic equipment.Product Features:High tear resist..
Flexural Modulus 0.600 - 0.600 GPa

@Temperature 90.0 - 90.0 °C
87.0 - 87.0 ksi

@Temperature 194 - 194 °F
Average value: 0.600 GPa Grade Count:1
Overview of materials for Nylon 6, Nucleated
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Nucleated". Each property range of values reported is minimum and maximum values of appropriate..