Mechanical Properties Metric English Comments
Flexural Modulus 5.52 - 6.07 GPa
800 - 880 ksi
Average value: 5.70 GPa Grade Count:3
Overview of materials for Nylon 11 with 30% Glass Fiber Filler
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 11 with 30% Glass Fiber Filler". Specific grades with glass content between 25% and 34% are includ..
Flexural Modulus 4.69 - 6.07 GPa
680 - 880 ksi
Bulk Molding Compounds BMC A50-EG Low Glass, Encapsulation Grade Molding Compound
BMC A50-EG is a low glass, encapsulation grade material. It is well suited for injection, transfer or compression molding of intricate parts. Typical applications are motor armatures and coils.Inf..