Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Bulk Molding Compounds BMC A50-EG Low Glass, Encapsulation Grade Molding Compound

Category Polymer , Thermoset , Polyester, TS , Thermoset Polyester Glass Filled BMC
Manufacturer BMC - Bulk Molding Compounds Inc.
Trade Name BMC
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Bulk Molding Compounds BMC A50-EG Low Glass, Encapsulation Grade Molding Compound.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
BMC A50-EG is a low glass, encapsulation grade material. It is well suited for injection, transfer or compression molding of intricate parts. Typical applications are motor armatures and coils.Information provided by Bulk Molding Compounds, Inc.
Physical Properties Metric English Comments
Density 1.55 - 1.75 g/cc
0.0560 - 0.0632 lb/in³
Molded
Linear Mold Shrinkage 0.00070 - 0.0017 cm/cm
0.00070 - 0.0017 in/in
Mechanical Properties Metric English Comments
Hardness, Barcol 45 - 50
45 - 50
Tensile Strength 49.0 - 62.7 MPa
7100 - 9100 psi
Flexural Strength 95.1 - 123 MPa
13800 - 17800 psi
Flexural Modulus 4.69 - 6.07 GPa
680 - 880 ksi
Compressive Strength 114 - 141 MPa
16500 - 20500 psi
Izod Impact, Notched 2.67 - 3.74 J/cm
5.00 - 7.00 ft-lb/in
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) >= 260 °C
>= 500 °F
Flammability, UL94 HB
HB
Electrical Properties Metric English Comments
Dielectric Strength 15.4 - 17.4 kV/mm
391 - 441 kV/in
short time
Arc Resistance >= 188 sec
>= 188 sec
Comparative Tracking Index >= 500 V
>= 500 V
Processing Properties Metric English Comments
Processing Temperature 138 - 166 °C
280 - 330 °F
Users viewing this material also viewed the following: