Polymer Property : Flexural Modulus = 891 ksi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Flexural Modulus 6.14 GPa
891 ksi
ASTM D790
PolyOne Trilliant™ HC HC3320-0020 RS Natural Polybutylene Terephthalate (PBT)
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead..
Flexural Modulus 6.14 GPa
891 ksi
ASTM D790
Omni Plastics OmniTech™ PA6/6 GR15 MS2 Wear-and-Friction Molybdenum Disulfide filled Nylon
OmniTech™ is a family of non-standard products custom developed for applications with unique functional requirements, including but not limited to: Flame Retardant, Conductive, Wear Resistant, and ..
Flexural Modulus 6.14 GPa
891 ksi
Clear Casting
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin
TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica..
Flexural Modulus 6.14 GPa
891 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOTUF VF006U Super Tough Nylon
LNP* Thermotuf* VF006U is a compound based on Super Tough Nylon containing Glass Fiber. Characteristics of this grade are High Impact.
Flexural Modulus 6.14 GPa
891 ksi
Clear Casting
TSE Industries EcoSPRAY® 350c Flame-Retardant Polyurethane Resin
TSE-EcoSPRAY® 350c is an “Environmentally-Preferred Product” or EPP. It is a Thixotropic flame retardant polyurethane resin free of Styrene, and is an “ultra-low” emitting resin during applica..