Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 2.30 - 9.74 GPa | 334 - 1410 ksi | Average value: 6.64 GPa Grade Count:10 |
Overview of materials for Polystyrene + Polyphenylene Ether, Glass + Mineral Filler This property data is a summary of similar materials in the MatWeb database for the category "Polystyrene + Polyphenylene Ether, Glass + Mineral Filler". Each property range of values reported is mi.. |