Mechanical Properties Metric English Comments
Flexural Modulus 6.39 GPa
927 ksi
ASTM D790
Plenco 50015 PET, Pellet, Injection Molded, White  (discontinued **)
PLENCO 50015 is an engineering grade glass reinforced polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL recognized and available in white, natu..
Flexural Modulus 6.39 GPa
927 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP THERMOCOMP DF004P PC (Asia Pacific)
LNP* Thermocomp* DF004P is a Polycarbonate base resin containing Glass Fiber. Characteristics of this grade are Exceptional Processing.