Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plenco 50015 PET, Pellet, Injection Molded, White  (discontinued **)

Category Polymer , Thermoplastic , Polyester, TP , Polyethylene Terephthalate (PET)
Manufacturer
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 50015 PET, Pellet, Injection Molded, White  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 50015 is an engineering grade glass reinforced polyethylene terephthalate resin designed for increased flexibility and good physical strength. It is UL recognized and available in white, natural, and black.Information supplied by PlencoPlenco discontinued their PET product line in 2005.
Physical Properties Metric English Comments
Density 1.47 g/cc
0.0531 lb/in³
ASTM D792
Water Absorption 0.060 %
0.060 %
ASTM D570
Linear Mold Shrinkage 0.0022 cm/cm
0.0022 in/in
ATM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 108.5 MPa
15740 psi
ASTM D638
Elongation at Break 1.9 %
1.9 %
ASTM D638
Tensile Modulus 6.26 GPa
908 ksi
ASTM D638
Flexural Yield Strength 151 MPa
21900 psi
ASTM D790
Flexural Modulus 6.39 GPa
927 ksi
ASTM D790
Compressive Yield Strength 150.4 MPa
21810 psi
ASTM D695
Izod Impact, Notched 0.450 J/cm
0.843 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 203 °C
397 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.47 mm
HB

@Thickness 0.0579 in
Electrical Properties Metric English Comments
Electrical Resistivity 4.26e+17 ohm-cm
4.26e+17 ohm-cm
ASTM D257
Dielectric Constant 2.9

@Frequency 1e+6 Hz
2.9

@Frequency 1e+6 Hz
ASTM D150
Dielectric Strength 15.9 kV/mm
404 kV/in
Short Time; ASTM D149
Dissipation Factor 0.015

@Frequency 1e+6 Hz
0.015

@Frequency 1e+6 Hz
ASTM D150
Arc Resistance 110 sec
110 sec
ASTM D495
Comparative Tracking Index 225 V
225 V
ASTM D3638