Mechanical Properties Metric English Comments
Flexural Modulus 0.641 GPa
93.0 ksi
At 2 mm/min; ASTM D790
Borealis Borecene™ RM7402 Linear Polyethylene for Rotational Molding
Borecene RM7402 is a third generation linear medium density natural polyethylene for rotational molding. The narrow molecular weight distribution imparted through metallocene catalyst technology pro..
Flexural Modulus 0.641 GPa
93.0 ksi
At 2 mm/min; ASTM D790
Borealis Borecene™ RM7403 Linear Polyethylene for Rotational Molding
Borecene Compact RM7403 is a third generation linear medium density black polyethylene for rotational molding. The narrow molecular weight imparted through metallocene catalyst technology provides ..
Flexural Modulus 0.641 GPa
93.0 ksi
2% secant; ASTM D790
ExxonMobil LL 6407.67 Injection Molding Resin
L Product Description: LL 6407 is a narrow molecular weight hexene copolymer designed for applications that require outstanding environmental stress crack resistance. This resin offers good processa..
Flexural Modulus 0.641 GPa
93.0 ksi
2% Secant; ASTM D638
ExxonMobil LLDPE LL 6407.67 Linear Low Density Polyethylene Resin
Product Description: LL 6407 is a narrow molecular weight hexene copolymer designed for applications that require outstanding environmental stress crack resistance. This resin offers good processabi..