ExxonMobil LL 6407.67 Injection Molding Resin

Category Polymer , Thermoplastic , Polyethylene (PE) , LLDPE , Linear Low Density Polyethylene (LLDPE), Injection Molded
Manufacturer Exxon Chemical
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF ExxonMobil LL 6407.67 Injection Molding Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
L Product Description: LL 6407 is a narrow molecular weight hexene copolymer designed for applications that require outstanding environmental stress crack resistance. This resin offers good processability with minimal warpage and outstanding toughness for cold temperature durability. Availability: Latin America, North America and South AmericaAdditive: Thermal Stabilizer: Yes Applications: Caps and ClosuresCargo handling boxesLarge LidsLarge Part Housewares Information provided by ExxonMobil Chemical
Physical Properties Metric English Comments
Density 0.936 g/cc
0.0338 lb/in³
ASTM D4883
Environmental Stress Crack Resistance 240 hour
240 hour
Condition B, 10%; ASTM D1693
Melt Flow 6.8 g/10 min

@Load 2.16 kg,
Temperature 190 °C
6.8 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 17.2 MPa
2500 psi
ASTM D638
Elongation at Break 1100 %
1100 %
ASTM D638
Flexural Modulus 0.641 GPa
93.0 ksi
2% secant; ASTM D790
Flexural Modulus, 1% Secant 758 MPa
110000 psi
Product Description: LL 6407 is a narrow molecular
Thermal Properties Metric English Comments
Melting Point 128 °C
262 °F
ASTM D3418
Vicat Softening Point 112 °C
234 °F
ASTM D1525
Descriptive Properties Value Comments
Features antioxidant thermal protection
Form PELLET