Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Flexural Modulus | 0.660 GPa | 95.7 ksi | ASTM D790 |
Nylene® PX1719 Nylon 6 Dry as molded. Extrusion grade. Nylene PX1719HS is a heat stabilized, high impact, nylon 6 extrusion grade resin with a low flexural modulus. PX1719HS is ideally suited for extrusion of tubing and.. |
|||
Flexural Modulus | 0.660 GPa | 95.7 ksi | 3 pt. secant. ASTM D790 |
Chevron Phillips HiD® 9638 HDPE Sheeting and Blown Film Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 225, A 56507Applications:Cast Geomembrane Applications, Notion and Millinery Bags, Heavy Duty Shipping Sacks, In.. |
|||
Flexural Modulus | 0.660 GPa | 95.7 ksi | 3 pt. secant. ASTM D790 |
Chevron Phillips HiD® 9642 HDPE Sheeting Resin
(discontinued **) Resin Type: Sheeting Resin for the Geomembrane Market; ASTM D 4976 Classification: PE 225, A 56507Applications:Blown Geomembrane Applications, Sanitary Landfill Liners, Waste Water Reservoir Contain.. |
|||
Flexural Modulus | 0.660 - 1.47 GPa | 95.7 - 213 ksi | Average value: 1.02 GPa Grade Count:10 |
Overview of materials for High Density Polyethylene (HDPE), Film Grade This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Film Grade". Each property range of values reported is minimum and max.. |
|||
Flexural Modulus | 0.660 GPa | 95.7 ksi | ISO 178 |
LyondellBasell Hostacomâ„¢ RE-44AC Thermoplastic Polyolefin Elastomer Description: Hostacomâ„¢ RE-44AC polypropylene TPO resin is a compounded product containing 25% minimum post-industrial or post-consumer recycled polypropylene and reactor grade thermoplastic ole.. |
|||
Flexural Modulus | 0.660 GPa | 95.7 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP TH0450A PUR LNP THERMOCOMP* TH0450A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Flexural Modulus | 0.660 GPa | 95.7 ksi | ASTM D790 |
SABIC Innovative Plastics LNP THERMOCOMP TH0450A PUR (Asia Pacific) LNP THERMOCOMP* TH0450A is a compound based on Polyurethane resin. Added features of this material include: High Specific Gravity. |
|||
Flexural Modulus | 0.660 GPa | 95.7 ksi | ASTM D790 |
Goodfellow TPX® MX002O Polymethylpentene This grade is highly recommended for injection molding, film and mandrel extrusion; also for fiber extrusion and blow molding.TPX® is semi-crystalline, transparent, very light and - for a polyolefi.. |
|||
Flexural Modulus | 0.660 GPa | 95.7 ksi | 2% Secant - 16:1 span:depth, 0.5 in/min; ASTM D-790 |
Chevron Phillips Marlex® HMN TR-938/938G Polyethylene; MDPE Medium density polyethylene. These hexene copolymers are tailored for rotational molding applications that require: Wide process windows and good flowLong-term UV stabilizationExcellent impact stre.. |