Mechanical Properties Metric English Comments
Flexural Modulus 6.79 GPa
985 ksi
ASTM D790
PolyOne Trilliantâ„¢ HC HC5220-0040 RS Natural Polypropylene, Unspecified (PP, Unspecified)
The Trilliant® specialty compounds offer a complete system of specialty engineered materials, certified processes, services and technical support that enable healthcare OEM's to get to market ahead..
Flexural Modulus 6.79 GPa
985 ksi
1.3 mm/min, 50 mm span; ASTM D790
SABIC Innovative Plastics LNP LUBRICOMP ZFL34 PPE+PS
LNP* LUBRICOMP* ZFL34 is a compound based on PPE+PS resin containing 20% Glass Fiber, 15% PTFE. Added feature of this gradae is: Wear Resistant.
Flexural Modulus 6.79 GPa
985 ksi
1.3 mm/min, 50 mm span; ASTM D 790
SABIC Innovative Plastics LNP Lubricomp ZFL34 PPO
LNP* Lubricomp* ZFL34 is a compound based on Modified PPO containing glass fiber and PTFE.This data was supplied by SABIC-IP for the Americas region.