Mechanical Properties Metric English Comments
Charpy Impact, Unnotched 213 J
157 ft-lb
1/2 size bar
Kinetics MIM 2.5% SiFe Soft Magnetic Steel
Low alloy steel, silicon. A work hardenable steel alloy that offers very good magnetic properties, tensile strength, hardness, wear resistance, and increased spring steel strength. Can be plated or ..