Mechanical Properties Metric English Comments
Charpy Impact, Unnotched 6.10 J
4.50 ft-lb
Pacific Sintered Materials FN-253-S(HT) 4600 Powdered Metal
High performance material with high strength and wear resistance after heat treatment.Equivalent MPIF Specification: FL-4605-100HTAll information provided by Pacific Sintered Metals.
Charpy Impact, Unnotched 6.10 J
4.50 ft-lb
PSM Industries Pacific Sintered Metals 4600 FN-253-S(HT) Powdered Metal
High performance material with high strength and wear resistance after heat treatment Equivalent MPIF Specification: FL-4605-100HTInformation Provided by Pacific Sintered Metals, a division of PSM ..
Charpy Impact, Unnotched 6.10 J
4.50 ft-lb
[ft-lb/in]; ASTM D256
CPC - Vycom CELTEC MARINE™ Expanded Foam PVC Polyvinyl Chloride
Celtec Marine is made from rigid expanded foam polyvinyl chloride (PVC) material whose combination of features makes it ideal for wood trim and plywood replacement in boat manufacturing. Its closed ..