Polymer Property : Puncture Energy = 9.20 J Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Puncture Energy 9.20 - 65.0 J
6.79 - 47.9 ft-lb
Average value: 37.7 J Grade Count:4
Overview of materials for Nylon 6, 40% Mineral Filled
This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of ap..
Puncture Energy 9.20 J
6.79 ft-lb
ISO 6603-2
Lanxess Durethan® BM 240 H2.0 901510 Nylon 6, 40% Mineral
PA 6, injection molding grade, 40% mineral, isotopic properties, good heat-ageing resistance