This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 40% Mineral Filled". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.29 - 1.61 g/cc
0.0466 - 0.0582 lb/in³
Average value: 1.46 g/cc Grade Count:65
1.28 - 1.28 g/cc

@Temperature >=250 °C
0.0462 - 0.0462 lb/in³

@Temperature >=482 °F
Average value: 1.28 g/cc Grade Count:1
Filler Content 35.0 - 40.0 %
35.0 - 40.0 %
Average value: 39.5 % Grade Count:17
Water Absorption 0.700 - 6.00 %
0.700 - 6.00 %
Average value: 2.37 % Grade Count:40
Moisture Absorption at Equilibrium 0.250 - 2.30 %
0.250 - 2.30 %
Average value: 1.62 % Grade Count:27
Water Absorption at Saturation 5.70 - 7.00 %
5.70 - 7.00 %
Average value: 6.07 % Grade Count:6
Linear Mold Shrinkage 0.00100 - 0.0180 cm/cm
0.00100 - 0.0180 in/in
Average value: 0.00743 cm/cm Grade Count:56
Linear Mold Shrinkage, Transverse 0.00200 - 0.0122 cm/cm
0.00200 - 0.0122 in/in
Average value: 0.00844 cm/cm Grade Count:13
Melt Flow 3.00 - 33.0 g/10 min
3.00 - 33.0 g/10 min
Average value: 19.0 g/10 min Grade Count:5
Mechanical Properties Metric English Comments
Hardness, Rockwell M 90.0 - 95.0
90.0 - 95.0
Average value: 93.3 Grade Count:3
Hardness, Rockwell R 103 - 122
103 - 122
Average value: 119 Grade Count:18
Ball Indentation Hardness 85.0 - 205 MPa
12300 - 29700 psi
Average value: 140 MPa Grade Count:3
Tensile Strength, Ultimate 35.0 - 137 MPa
5080 - 19900 psi
Average value: 72.8 MPa Grade Count:45
20.0 - 135 MPa

@Temperature -40.0 - 120 °C
2900 - 19600 psi

@Temperature -40.0 - 248 °F
Average value: 62.1 MPa Grade Count:7
Tensile Strength, Yield 45.0 - 120 MPa
6530 - 17400 psi
Average value: 82.5 MPa Grade Count:26
20.0 - 90.0 MPa

@Temperature -40.0 - 120 °C
2900 - 13100 psi

@Temperature -40.0 - 248 °F
Average value: 45.0 MPa Grade Count:1
Elongation at Break 1.50 - 40.0 %
1.50 - 40.0 %
Average value: 14.6 % Grade Count:50
5.00 - 40.0 %

@Temperature -40.0 - 120 °C
5.00 - 40.0 %

@Temperature -40.0 - 248 °F
Average value: 25.6 % Grade Count:3
Elongation at Yield 2.50 - 27.0 %
2.50 - 27.0 %
Average value: 7.84 % Grade Count:16
5.10 - 30.0 %

@Temperature -40.0 - 120 °C
5.10 - 30.0 %

@Temperature -40.0 - 248 °F
Average value: 20.0 % Grade Count:1
Modulus of Elasticity 2.00 - 7.58 GPa
290 - 1100 ksi
Average value: 4.70 GPa Grade Count:32
0.600 - 8.31 GPa

@Temperature -40.0 - 150 °C
87.0 - 1210 ksi

@Temperature -40.0 - 302 °F
Average value: 3.50 GPa Grade Count:5
Flexural Yield Strength 50.0 - 250 MPa
7250 - 36300 psi
Average value: 117 MPa Grade Count:50
25.0 - 207 MPa

@Temperature -40.0 - 120 °C
3630 - 30000 psi

@Temperature -40.0 - 248 °F
Average value: 84.2 MPa Grade Count:6
Flexural Modulus 1.50 - 7.88 GPa
218 - 1140 ksi
Average value: 5.13 GPa Grade Count:56
0.700 - 8.60 GPa

@Temperature -40.0 - 120 °C
102 - 1250 ksi

@Temperature -40.0 - 248 °F
Average value: 2.76 GPa Grade Count:7
Compressive Yield Strength 69.0 - 186 MPa
10000 - 27000 psi
Average value: 124 MPa Grade Count:5
Izod Impact, Notched 0.267 - 100 J/cm
0.500 - 187 ft-lb/in
Average value: 0.664 J/cm Grade Count:36
0.320 - 0.820 J/cm

@Temperature -40.0 - -40.0 °C
0.599 - 1.54 ft-lb/in

@Temperature -40.0 - -40.0 °F
Average value: 0.578 J/cm Grade Count:3
Izod Impact, Unnotched 0.374 - 16.4 J/cm
0.700 - 30.7 ft-lb/in
Average value: 5.72 J/cm Grade Count:9
Izod Impact, Notched (ISO) 3.90 - 10.0 kJ/m²
1.86 - 4.76 ft-lb/in²
Average value: 7.17 kJ/m² Grade Count:8
4.00 - 10.0 kJ/m²

@Temperature -40.0 - -20.0 °C
1.90 - 4.76 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 7.31 kJ/m² Grade Count:4
Izod Impact, Unnotched (ISO) 100 kJ/m² - NB
47.6 ft-lb/in² - NB
Average value: 117 kJ/m² Grade Count:3
75.0 - 85.0 kJ/m²

@Temperature -30.0 - -30.0 °C
35.7 - 40.4 ft-lb/in²

@Temperature -22.0 - -22.0 °F
Average value: 80.0 kJ/m² Grade Count:2
Charpy Impact Unnotched 1.70 J/cm² - NB
8.09 ft-lb/in² - NB
Average value: 9.57 J/cm² Grade Count:21
1.80 J/cm² - NB

@Temperature -40.0 - -20.0 °C
8.57 ft-lb/in² - NB

@Temperature -40.0 - -4.00 °F
Average value: 7.38 J/cm² Grade Count:8
Charpy Impact, Notched 0.300 - 1.20 J/cm²
1.43 - 5.71 ft-lb/in²
Average value: 0.730 J/cm² Grade Count:22
0.270 - 1.00 J/cm²

@Temperature -40.0 - -20.0 °C
1.28 - 4.76 ft-lb/in²

@Temperature -40.0 - -4.00 °F
Average value: 0.734 J/cm² Grade Count:10
Puncture Energy 9.20 - 65.0 J
6.79 - 47.9 ft-lb
Average value: 37.7 J Grade Count:4
1.60 - 3.00 J

@Temperature -30.0 - -30.0 °C
1.18 - 2.21 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 2.65 J Grade Count:2
3.00 - 3.00 J

@Temperature -30.0 - -30.0 °C
2.21 - 2.21 ft-lb

@Temperature -22.0 - -22.0 °F
Average value: 2.65 J Grade Count:2
3.00 - 3.00 J

@Load <=74.2 kg
2.21 - 2.21 ft-lb

@Load <=164 lb
Average value: 2.65 J Grade Count:2
Thermal Properties Metric English Comments
CTE, linear 7.20 - 74.0 µm/m-°C
4.00 - 41.1 µin/in-°F
Average value: 49.9 µm/m-°C Grade Count:28
CTE, linear, Transverse to Flow 58.0 - 75.0 µm/m-°C
32.2 - 41.7 µin/in-°F
Average value: 66.1 µm/m-°C Grade Count:8
Specific Heat Capacity 1.94 - 2.00 J/g-°C
0.464 - 0.478 BTU/lb-°F
Average value: 1.99 J/g-°C Grade Count:6
Electrical Properties Metric English Comments
Electrical Resistivity 1.00e+9 - 1.00e+16 ohm-cm
1.00e+9 - 1.00e+16 ohm-cm
Average value: 8.66e+14 ohm-cm Grade Count:24
Surface Resistance 1.00e+10 - 1.00e+14 ohm
1.00e+10 - 1.00e+14 ohm
Average value: 3.04e+13 ohm Grade Count:7
Dielectric Constant 3.60 - 15.0
3.60 - 15.0
Average value: 5.63 Grade Count:9
Dielectric Strength 16.0 - 42.1 kV/mm
406 - 1070 kV/in
Average value: 26.3 kV/mm Grade Count:16
Dissipation Factor 0.0110 - 0.250
0.0110 - 0.250
Average value: 0.0597 Grade Count:8
Arc Resistance 115 - 190 sec
115 - 190 sec
Average value: 138 sec Grade Count:6
Comparative Tracking Index 400 - 600 V
400 - 600 V
Average value: 525 V Grade Count:12
Users viewing this material also viewed the following: